species namemoisture contentcategorycompression parallel kPa (kPa)compression perpendicular kPa (kPa)impact bending mm (mm)modulus of elasticity MPa (MPa)modulus of rupture kPa (kPa)originradial shrinkage pct (%)shear parallel kPa (kPa)side hardness N (N)specific gravity (dimensionless)tangential shrinkage pct (%)tension perpendicular kPa (kPa)thermal conductivity W mK (W/(m·K))volumetric shrinkage pct (%)work to max load kJ m3 (kJ/m3)
Tupelo, Water12%Hardwood40,8006,0005808,70066,000Domestic4.211,0003,9000.57.64,8000.1512.548
Tupelo, WaterGreenHardwood23,2003,3007607,20050,000Domestic4.28,2003,2000.467.64,1000.1212.557