Sample data from Engineering Database — 375 reference tables, deterministic calculators, and Engineering AI. Sign up free

Thermal Conductivity Vs Temperature: silicon dioxide polycrystalline

-173 to 927

Temperature-dependent thermal conductivity for engineering materials — metals, alloys, ceramics, semiconductors, and polymers from -275C to 2300C

Mechanical Engineeringmaterial: silicon dioxide polycrystalline7 rows
materialtemperature Cmaterial categorythermal conductivity WmK (W/mK)
silicon dioxide polycrystalline-173Ceramic0.69
silicon dioxide polycrystalline-73Ceramic1.14
silicon dioxide polycrystalline127Ceramic1.51
silicon dioxide polycrystalline327Ceramic1.75
silicon dioxide polycrystalline527Ceramic2.17
silicon dioxide polycrystalline727Ceramic2.87
silicon dioxide polycrystalline927Ceramic4