Thermal Conductivity Vs Temperature: graphite_pyrolytic_perp
Temperature-dependent thermal conductivity for engineering materials — metals, alloys, ceramics, semiconductors, and polymers from -275C to 2300C
| material | temperature C | material category | thermal conductivity WmK (W/mK) |
|---|---|---|---|
| graphite_pyrolytic_perp | -173 | Carbon | 16.8 |
| graphite_pyrolytic_perp | -73 | Carbon | 9.23 |
| graphite_pyrolytic_perp | 127 | Carbon | 4.09 |
This is a sample. Search the full thermal conductivity vs temperature dataset and 350+ more by creating a free account and accessing the database.
Get started for FREE