Spring Wire Data: Hastelloy C-276 Wire AMS B574 (Chem. only), AMS J470 UNS N10276 to Inconel 718 Spring Tempered Wire ASTM B637 UNS N07718
Spring wire material data — tensile strength ranges, working temperatures, and elastic moduli for common spring wire materials (music wire, chrome vanadium, stainless, etc.)
| material | approx design of ultimate tensile torsional | common sizes in | dataset | material properties | maximum working temp | modulus of elasticity psi 106 | source page | source table idx | ultimate tensile range ksi |
|---|---|---|---|---|---|---|---|---|---|
| Hastelloy C-276 Wire AMS B574 (Chem. only), AMS J470 UNS N10276 | - | .012" to .437" | spring_wire_data | Good corrosion resistance to many acids and salts. | see comment | (E) 29.8 (G) 10.9 | 33 | 0 | see comment |
| Inconel 600 QQ-W-390 UNS N06600 | 45% | .005" to .750" | spring_wire_data | Cold drawn. Good corrosion resistance. Good for use in elevated temperature applications. | 700°F | (E) 29 G) 11.0 | 25 | 0 | 205/120 |
| Inconel 625 Spring Tempered Wire ASTM B446 UNS N06625 | 45% | .012" to .175" | spring_wire_data | Cold drawn. Good corrosion resistance. Good for use in elevated temperature applications. | - | (E) 29 (G) 11.0 | 26 | 0 | 120 |
| Inconel 718 Bar ASTM B637 UNS N07718 | 45% | .234" to 1.500" | spring_wire_data | Age hardened. Good corrosion resistance. Good for use in elevated temperature applications. No magnetism. | 1200°F | (E) 29 (G) 11.2 | 28 | 0 | 250/210 |
| Inconel 718 Spring Tempered Wire ASTM B637 UNS N07718 | 45% | .012" to .275" | spring_wire_data | Age hardened. Good corrosion resistance. Good for use in elevated temperature applications. No magnetism | 1200°F | (E) 29 (G) 11.2 | 27 | 0 | 250/210 |