Zamak-7-AG40B-Die-Cast — Zinc Alloy

Category
Zinc Alloy
Material Id
Zamak 7 AG40B Die Cast
Brinell Hardness (HB)
80
Cte per K (1/K)
0.000027
Density Kg M3 (kg/m3)
6,600
Elastic Modulus MPa (MPa)
85,000
Elongation Percent (%)
13
Grade
AG40B
Heat Treatment
Die Cast
Melting Point C (°C)
384
Name
Zamak 7 (Zn-4Al-0.4Mg Low-impurity)
Specific Heat J kgK (J/(kg·K))
419
Standard
ASTM B86
Tensile Strength MPa (MPa)
283
Thermal Conductivity W mK (W/(m·K))
113
Yield Strength MPa (MPa)
221

Source: ASTM B86