SAE-446-Stainless-Steel-Annealed-at-815-C-1500-F-and-Cold-Drawn — Stainless Steel

Category
Stainless Steel
Material Id
SAE 446 Stainless Steel Annealed at 815 °C 1500 °F and Cold Drawn
Brinell Hardness (HB)
216
Cte per K (1/K)
0.000011
Density Kg M3 (kg/m3)
7,850
Elastic Modulus MPa (MPa)
193,000
Elongation Percent (%)
26
Grade
446
Heat Treatment
Annealed at 815 °C (1500 °F) and Cold Drawn
Melting Point C (°C)
1,480
Name
SAE 446 Stainless Steel (Annealed at 815 °C (1500 °F) and Cold drawn)
Poisson Ratio (dimensionless)
0.3
Reduction Percent (%)
64
Shear Modulus MPa (MPa)
74,230.8
Specific Heat J kgK (J/(kg·K))
460
Standard
SAE
Tensile Strength MPa (MPa)
607
Thermal Conductivity W mK (W/(m·K))
25
Yield Strength MPa (MPa)
462