SAE-440C-Stainless-Steel-Annealed-and-Cold-Drawn-Bar — Stainless Steel

Category
Stainless Steel
Material Id
SAE 440C Stainless Steel Annealed and Cold Drawn Bar
Brinell Hardness (HB)
260
Cte per K (1/K)
0.00001
Density Kg M3 (kg/m3)
7,850
Elastic Modulus MPa (MPa)
193,000
Elongation Percent (%)
7
Grade
440C
Heat Treatment
Annealed and Cold Drawn Bar
Melting Point C (°C)
1,450
Name
SAE 440C Stainless Steel (Annealed and Cold Drawn bar)
Poisson Ratio (dimensionless)
0.3
Reduction Percent (%)
20
Shear Modulus MPa (MPa)
74,230.8
Specific Heat J kgK (J/(kg·K))
460
Standard
SAE
Tensile Strength MPa (MPa)
860
Thermal Conductivity W mK (W/(m·K))
24.7
Yield Strength MPa (MPa)
690

Source: SAE