Explore the Engineering Database more efficiently by signing up for free. Sign up free
Home/Reference Data/Metal Alloy Properties/Stainless Steel/SAE-431-Stainless-Steel-Oil-quenched-from-980-C-1800-F-tempered-at-650-C-120

SAE-431-Stainless-Steel-Oil-Quenched-From-980-C-1800-F-Tempered-at-650-C-120 — Stainless Steel

Category
Stainless Steel
Material Id
SAE 431 Stainless Steel Oil Quenched From 980 °C 1800 °F; Tempered at 650 °C 1200
Cte per K (1/K)
0.00001
Density Kg M3 (kg/m3)
7,850
Elastic Modulus MPa (MPa)
193,000
Elongation Percent (%)
20
Grade
431
Heat Treatment
Oil Quenched From 980 °C (1800 °F); Tempered at 650 °C (1200 °F)
Melting Point C (°C)
1,450
Name
SAE 431 Stainless Steel (Oil Quenched From 980 °C (1800 °F); Tempered at 650 °C (1200)
Poisson Ratio (dimensionless)
0.3
Reduction Percent (%)
64
Shear Modulus MPa (MPa)
74,230.8
Specific Heat J kgK (J/(kg·K))
460
Standard
SAE
Tensile Strength MPa (MPa)
831
Thermal Conductivity W mK (W/(m·K))
24.7
Yield Strength MPa (MPa)
738

Source: SAE

stainless_steel — material id SAE_431_Stainless_Steel_Oil_quenched_from_980_°C_1800_°F; tempered_at_650_°C_120… · name SAE 431 Stainless Steel (Oil quenched from 980 °C (1800 °F); tempered at 650 °C… · tensile strength MPa 831 MPa · yield strength MPa 738 MPa · grade 431 | Metal Alloy Properties | Engineering Database