Explore the Engineering Database more efficiently by signing up for free. Sign up free
Home/Reference Data/Metal Alloy Properties/Stainless Steel/SAE-420-Stainless-Steel-Annealed-and-cold-drawn

SAE-420-Stainless-Steel-Annealed-and-Cold-Drawn — Stainless Steel

Category
Stainless Steel
Material Id
SAE 420 Stainless Steel Annealed and Cold Drawn
Brinell Hardness (HB)
228
Cte per K (1/K)
0.00001
Density Kg M3 (kg/m3)
7,850
Elastic Modulus MPa (MPa)
193,000
Elongation Percent (%)
14
Grade
420
Heat Treatment
Annealed and Cold Drawn
Melting Point C (°C)
1,450
Name
SAE 420 Stainless Steel (Annealed and Cold drawn)
Poisson Ratio (dimensionless)
0.3
Reduction Percent (%)
40
Shear Modulus MPa (MPa)
74,230.8
Specific Heat J kgK (J/(kg·K))
460
Standard
SAE
Tensile Strength MPa (MPa)
760
Thermal Conductivity W mK (W/(m·K))
24.7
Yield Strength MPa (MPa)
690

Source: SAE

stainless_steel — material id SAE_420_Stainless_Steel_Annealed_and_cold_drawn · name SAE 420 Stainless Steel (Annealed and cold drawn) · tensile strength MPa 760 MPa · yield strength MPa 690 MPa · grade 420 | Metal Alloy Properties | Engineering Database