Explore the Engineering Database more efficiently by signing up for free. Sign up free

Ati-EBrite-Annealed — Stainless Steel

Category
Stainless Steel
Material Id
Ati EBrite Annealed
Cte per K (1/K)
0.00001
Density Kg M3 (kg/m3)
7,600
Elastic Modulus MPa (MPa)
200,000
Elongation Percent (%)
30
Grade
UNS S44627
Heat Treatment
Annealed
Name
Ati E-Brite Superferritic Stainless Steel
Property Basis
Typical
Specific Heat J kgK (J/(kg·K))
427
Standard
ASTM A240 (XM-27)
Tensile Strength MPa (MPa)
485
Test Direction
Longitudinal
Thermal Conductivity W mK (W/(m·K))
16.7
Yield Strength MPa (MPa)
345

Source: ASTM A240 (XM-27)

stainless_steel — material id ATI_EBrite_Annealed · name ATI E-Brite Superferritic Stainless Steel · tensile strength MPa 485 MPa · yield strength MPa 345 MPa · grade UNS S44627 | Metal Alloy Properties | Engineering Database