Explore the Engineering Database more efficiently by signing up for free. Sign up free

Ati-316LN-Annealed — Stainless Steel

Category
Stainless Steel
Material Id
Ati 316LN Annealed
Brinell Hardness (HB)
217
Cte per K (1/K)
0.000017
Density Kg M3 (kg/m3)
8,000
Elastic Modulus MPa (MPa)
193,000
Elongation Percent (%)
40
Grade
316LN
Heat Treatment
Annealed
Melting Point C (°C)
1,345
Name
Ati 316LN Austenitic Stainless Steel (Low Carbon, Nitrogen Enhanced)
Property Basis
Minimum
Standard
ASTM A240
Tensile Strength MPa (MPa)
515
Thermal Conductivity W mK (W/(m·K))
14.6
Yield Strength MPa (MPa)
205

Source: ASTM A240