Explore the Engineering Database more efficiently by signing up for free. Sign up free

Ati-316L-Annealed — Stainless Steel

Category
Stainless Steel
Material Id
Ati 316L Annealed
Brinell Hardness (HB)
217
Cte per K (1/K)
0.000017
Density Kg M3 (kg/m3)
8,027
Elastic Modulus MPa (MPa)
200,000
Elongation Percent (%)
40
Grade
316L
Heat Treatment
Annealed
Melting Point C (°C)
1,390
Name
Ati 316L Austenitic Stainless Steel (Low Carbon, Mo-bearing)
Property Basis
Minimum
Shear Modulus MPa (MPa)
82,000
Specific Heat J kgK (J/(kg·K))
460
Standard
ASTM A240
Tensile Strength MPa (MPa)
485
Thermal Conductivity W mK (W/(m·K))
14.6
Yield Strength MPa (MPa)
170

Source: ASTM A240