Ati-304L-Annealed — Stainless Steel

Category
Stainless Steel
Material Id
Ati 304L Annealed
Brinell Hardness (HB)
201
Cte per K (1/K)
0.000017
Density Kg M3 (kg/m3)
7,900
Elastic Modulus MPa (MPa)
200,000
Elongation Percent (%)
40
Grade
304L
Heat Treatment
Annealed
Melting Point C (°C)
1,399
Name
Ati 304L Austenitic Stainless Steel (Low Carbon)
Property Basis
Minimum
Specific Heat J kgK (J/(kg·K))
460
Standard
ASTM A240
Tensile Strength MPa (MPa)
485
Thermal Conductivity W mK (W/(m·K))
16.3
Yield Strength MPa (MPa)
170

Source: ASTM A240