Ati-201LHP-Annealed — Stainless Steel
- Category
- Stainless Steel
- Material Id
- Ati 201LHP Annealed
- Cte per K (1/K)
- 0.000017
- Density Kg M3 (kg/m3)
- 7,860
- Elastic Modulus MPa (MPa)
- 207,000
- Elongation Percent (%)
- 56
- Grade
- 201L Hp
- Heat Treatment
- Annealed
- Melting Point C (°C)
- 1,400
- Name
- Ati 201L Hp Austenitic Stainless Steel (Low Carbon)
- Property Basis
- Typical
- Rockwell B Hardness (HRB)
- 93
- Specific Heat J kgK (J/(kg·K))
- 460
- Standard
- ASTM A240
- Tensile Strength MPa (MPa)
- 785
- Test Direction
- Longitudinal
- Thermal Conductivity W mK (W/(m·K))
- 16.3
- Yield Strength MPa (MPa)
- 396
Source: ASTM A240