Explore the Engineering Database more efficiently by signing up for free. Sign up free

Ati-20-Plate-Annealed-Typical — Stainless Steel

Category
Stainless Steel
Material Id
Ati 20 Plate Annealed Typical
Brinell Hardness (HB)
210
Cte per K (1/K)
0.000015
Density Kg M3 (kg/m3)
8,080
Elastic Modulus MPa (MPa)
193,000
Elongation Percent (%)
40
Grade
UNS N08020
Heat Treatment
Annealed
Name
Ati 20 (Superaustenitic)
Property Basis
Typical
Specific Heat J kgK (J/(kg·K))
460
Standard
ASTM B463
Tensile Strength MPa (MPa)
621
Test Direction
Longitudinal
Thermal Conductivity W mK (W/(m·K))
12.2
Yield Strength MPa (MPa)
380

Source: ASTM B463

stainless_steel — material id ATI_20_Plate_Annealed_Typical · name ATI 20 (Superaustenitic) · tensile strength MPa 621 MPa · yield strength MPa 380 MPa · grade UNS N08020 | Metal Alloy Properties | Engineering Database