Explore the Engineering Database more efficiently by signing up for free. Sign up free

Ati-15-7-Condition-a — Stainless Steel

Category
Stainless Steel
Material Id
Ati 15-7 Condition a
Cte per K (1/K)
0.000014
Density Kg M3 (kg/m3)
7,800
Elastic Modulus MPa (MPa)
195,000
Elongation Percent (%)
30
Grade
UNS S15700
Heat Treatment
Condition a (Solution Annealed)
Name
Ati 15-7 Ph (Semi-Austenitic)
Property Basis
Typical
Standard
AMS 5520
Tensile Strength MPa (MPa)
860
Test Direction
Longitudinal
Yield Strength MPa (MPa)
380

Source: AMS 5520