317LMN-Annealed — Stainless Steel

Category
Stainless Steel
Material Id
317LMN Annealed
Cte per K (1/K)
0.000016
Density Kg M3 (kg/m3)
8,000
Elastic Modulus MPa (MPa)
200,000
Elongation Percent (%)
40
Grade
S31726
Heat Treatment
Annealed
Melting Point C (°C)
1,443
Name
317LMN Austenitic
Specific Heat J kgK (J/(kg·K))
460
Standard
ASTM A240
Tensile Strength MPa (MPa)
550
Thermal Conductivity W mK (W/(m·K))
14
Yield Strength MPa (MPa)
205

Source: ASTM A240