Explore the Engineering Database more efficiently by signing up for free. Sign up free

Meteorite-Iron-Taenite — Pure Metal

Category
Pure Metal
Material Id
Meteorite Iron Taenite
Cte per K (1/K)
0.000013
Density Kg M3 (kg/m3)
8,000
Elastic Modulus MPa (MPa)
185,000
Elongation Percent (%)
8
Grade
Fe-30Ni Gamma Phase (taenite)
Heat Treatment
Meteoritic (very Slow cooled)
Melting Point C (°C)
1,450
Name
Meteorite Iron Taenite (Fe-30Ni)
Standard
Buchwald "Handbook of Iron Meteorites" (1975) / Smithells Metals Reference Book
Tensile Strength MPa (MPa)
700
Thermal Conductivity W mK (W/(m·K))
18
Yield Strength MPa (MPa)
400

Source: Buchwald "Handbook of Iron Meteorites" (1975) / Smithells Metals Reference Book

pure_metal — material id Meteorite_Iron_Taenite · name Meteorite Iron Taenite (Fe-30Ni) · grade Fe-30Ni gamma phase (taenite) · elastic modulus MPa 185000 MPa · density kg m3 8000 kg/m3 | Metal Alloy Properties | Engineering Database