Steel-25-Gost-1050-88-Gost-Cold-Working — Carbon Steel

Category
Carbon Steel
Material Id
Steel 25 Gost 1050-88 Gost Cold Working
Brinell Hardness (HB)
217
Cte per K (1/K)
0.000012
Density Kg M3 (kg/m3)
7,820
Elastic Modulus MPa (MPa)
198,000
Elongation Percent (%)
7
Heat Treatment
Cold Working
Melting Point C (°C)
1,480
Name
Steel 25 Gost 1050-88
Poisson Ratio (dimensionless)
0.29
Shear Modulus MPa (MPa)
77,000
Specific Heat J kgK (J/(kg·K))
458
Standard
Gost
Tensile Strength MPa (MPa)
540
Thermal Conductivity W mK (W/(m·K))
63.5
Yield Strength MPa (MPa)
350

Source: GOST

carbon_steel — material id Steel_25_GOST_1050-88_GOST_Cold_working · name Steel 25 GOST 1050-88 · tensile strength MPa 540 MPa · yield strength MPa 350 MPa | Metal Alloy Properties | Engineering Database