Steel-20G-Gost-1050-88-Gost-Quenching-and-Cooling-in-the-Water — Carbon Steel
- Category
- Carbon Steel
- Material Id
- Steel 20G Gost 1050-88 Gost Quenching and Cooling in the Water
- Cte per K (1/K)
- 0.000012
- Density Kg M3 (kg/m3)
- 7,820
- Elastic Modulus MPa (MPa)
- 204,000
- Heat Treatment
- Quenching and Cooling in the Water
- Melting Point C (°C)
- 1,480
- Name
- Steel 20G Gost 1050-88
- Poisson Ratio (dimensionless)
- 0.29
- Shear Modulus MPa (MPa)
- 79,000
- Specific Heat J kgK (J/(kg·K))
- 457
- Standard
- Gost
- Tensile Strength MPa (MPa)
- 570
- Thermal Conductivity W mK (W/(m·K))
- 65.4
- Yield Strength MPa (MPa)
- 420
Source: GOST