SAE-1025-Carbon-Steel-Hot-Rolled — Carbon Steel

Category
Carbon Steel
Material Id
SAE 1025 Carbon Steel Hot Rolled
Brinell Hardness (HB)
116
Cte per K (1/K)
0.000012
Density Kg M3 (kg/m3)
7,850
Elastic Modulus MPa (MPa)
200,000
Elongation Percent (%)
25
Grade
1025
Heat Treatment
Hot Rolled
Melting Point C (°C)
1,480
Name
SAE 1025 Carbon Steel (Hot rolled)
Poisson Ratio (dimensionless)
0.3
Reduction Percent (%)
50
Shear Modulus MPa (MPa)
76,923.1
Specific Heat J kgK (J/(kg·K))
458
Standard
SAE
Tensile Strength MPa (MPa)
400
Thermal Conductivity W mK (W/(m·K))
63.5
Yield Strength MPa (MPa)
220

Source: SAE