DIN-X6Cr17 — Carbon Steel

Category
Carbon Steel
Material Id
DIN X6Cr17
Cte per K (1/K)
0.000012
Density Kg M3 (kg/m3)
7,860
Elastic Modulus MPa (MPa)
206,000
Elongation Percent (%)
20
Melting Point C (°C)
1,480
Name
DIN X6Cr17
Poisson Ratio (dimensionless)
0.3
Shear Modulus MPa (MPa)
80,000
Specific Heat J kgK (J/(kg·K))
460
Standard
DIN
Tensile Strength MPa (MPa)
450
Thermal Conductivity W mK (W/(m·K))
51.9
Yield Strength MPa (MPa)
270

Source: DIN