Explore the Engineering Database more efficiently by signing up for free. Sign up free

DIN-37Cr4-DIN-Heat-Treated — Carbon Steel

Category
Carbon Steel
Material Id
DIN 37Cr4 DIN Heat Treated
Cte per K (1/K)
0.000012
Density Kg M3 (kg/m3)
7,860
Elastic Modulus MPa (MPa)
206,000
Elongation Percent (%)
13
Heat Treatment
Heat Treated
Melting Point C (°C)
1,480
Name
DIN 37Cr4
Poisson Ratio (dimensionless)
0.3
Shear Modulus MPa (MPa)
80,000
Specific Heat J kgK (J/(kg·K))
462
Standard
DIN
Tensile Strength MPa (MPa)
850
Thermal Conductivity W mK (W/(m·K))
58.9
Vickers Hardness (HV)
270
Yield Strength MPa (MPa)
630

Source: DIN

carbon_steel — material id DIN_37Cr4_DIN_heat_treated · name DIN 37Cr4 · tensile strength MPa 850 MPa · yield strength MPa 630 MPa | Metal Alloy Properties | Engineering Database