Explore the Engineering Database more efficiently by signing up for free. Sign up free

Bs-708M40-Bs-Heat-Treated — Carbon Steel

Category
Carbon Steel
Material Id
Bs 708M40 Bs Heat Treated
Cte per K (1/K)
0.000012
Density Kg M3 (kg/m3)
7,860
Elastic Modulus MPa (MPa)
206,000
Elongation Percent (%)
13
Heat Treatment
Heat Treated
Melting Point C (°C)
1,480
Name
Bs 708M40
Poisson Ratio (dimensionless)
0.3
Shear Modulus MPa (MPa)
80,000
Specific Heat J kgK (J/(kg·K))
462
Standard
Bs
Tensile Strength MPa (MPa)
850
Thermal Conductivity W mK (W/(m·K))
51.9
Yield Strength MPa (MPa)
665

Source: BS

carbon_steel — material id BS_708M40_BS_heat_treated · name BS 708M40 · tensile strength MPa 850 MPa · yield strength MPa 665 MPa | Metal Alloy Properties | Engineering Database