Aluminum-Alloy-7075-T6 — Aluminum Alloy
- Category
- Aluminum Alloy
- Material Id
- Aluminum Alloy 7075-T6
- Brinell Hardness (HB)
- 150
- Cte per K (1/K)
- 0.000024
- Density Kg M3 (kg/m3)
- 2,700
- Elastic Modulus MPa (MPa)
- 73,000
- Elongation Percent (%)
- 11
- Heat Treatment
- Wrought
- Melting Point C (°C)
- 477
- Name
- Aluminum Alloy 7075-T6
- Poisson Ratio (dimensionless)
- 0.33
- Property Basis
- Typical
- Shear Modulus MPa (MPa)
- 26,000
- Specific Heat J kgK (J/(kg·K))
- 860
- Standard
- ANSI
- Tensile Strength MPa (MPa)
- 572
- Thermal Conductivity W mK (W/(m·K))
- 130
- Yield Strength MPa (MPa)
- 503
Source: ANSI