Explore the Engineering Database more efficiently by signing up for free. Sign up free

Aluminum-Alloy-6351-T6 — Aluminum Alloy

Category
Aluminum Alloy
Material Id
Aluminum Alloy 6351-T6
Brinell Hardness (HB)
95
Cte per K (1/K)
0.000023
Density Kg M3 (kg/m3)
2,700
Elastic Modulus MPa (MPa)
73,000
Elongation Percent (%)
14
Heat Treatment
Wrought
Melting Point C (°C)
582
Name
Aluminum Alloy 6351-T6
Poisson Ratio (dimensionless)
0.33
Shear Modulus MPa (MPa)
26,000
Specific Heat J kgK (J/(kg·K))
896
Standard
ANSI
Tensile Strength MPa (MPa)
310
Thermal Conductivity W mK (W/(m·K))
167
Yield Strength MPa (MPa)
283

Source: ANSI