Aluminum-Alloy-5652-H36 — Aluminum Alloy

Category
Aluminum Alloy
Material Id
Aluminum Alloy 5652-H36
Brinell Hardness (HB)
73
Cte per K (1/K)
0.000024
Density Kg M3 (kg/m3)
2,700
Elastic Modulus MPa (MPa)
73,000
Elongation Percent (%)
8
Heat Treatment
Wrought
Melting Point C (°C)
568
Name
Aluminum Alloy 5652-H36
Poisson Ratio (dimensionless)
0.33
Shear Modulus MPa (MPa)
26,000
Specific Heat J kgK (J/(kg·K))
880
Standard
ANSI
Tensile Strength MPa (MPa)
276
Thermal Conductivity W mK (W/(m·K))
117
Yield Strength MPa (MPa)
241

Source: ANSI