Aluminum-Alloy-328.0-ANSI-Cast-T6 — Aluminum Alloy

Category
Aluminum Alloy
Material Id
Aluminum Alloy 328.0 ANSI Cast T6
Brinell Hardness (HB)
65
Cte per K (1/K)
0.000021
Density Kg M3 (kg/m3)
2,700
Elastic Modulus MPa (MPa)
73,000
Elongation Percent (%)
1
Heat Treatment
Cast (T6)
Melting Point C (°C)
521
Name
Aluminum Alloy 328.0
Poisson Ratio (dimensionless)
0.33
Shear Modulus MPa (MPa)
26,000
Specific Heat J kgK (J/(kg·K))
900
Standard
ANSI
Tensile Strength MPa (MPa)
234
Thermal Conductivity W mK (W/(m·K))
155
Yield Strength MPa (MPa)
145

Source: ANSI