Explore the Engineering Database more efficiently by signing up for free. Sign up free

Aluminum-Alloy-3004-H38 — Aluminum Alloy

Category
Aluminum Alloy
Material Id
Aluminum Alloy 3004-H38
Brinell Hardness (HB)
77
Cte per K (1/K)
0.000023
Density Kg M3 (kg/m3)
2,700
Elastic Modulus MPa (MPa)
73,000
Elongation Percent (%)
5
Heat Treatment
Wrought
Melting Point C (°C)
629
Name
Aluminum Alloy 3004-H38
Poisson Ratio (dimensionless)
0.33
Shear Modulus MPa (MPa)
26,000
Specific Heat J kgK (J/(kg·K))
893
Standard
ANSI
Tensile Strength MPa (MPa)
283
Thermal Conductivity W mK (W/(m·K))
159
Yield Strength MPa (MPa)
248

Source: ANSI

aluminum_alloy — material id Aluminum_Alloy_3004-H38 · name Aluminum Alloy 3004-H38 · tensile strength MPa 283 MPa · yield strength MPa 248 MPa · elongation percent 5 % | Metal Alloy Properties | Engineering Database