Aluminum-Alloy-2011-T3 — Aluminum Alloy

Category
Aluminum Alloy
Material Id
Aluminum Alloy 2011-T3
Brinell Hardness (HB)
95
Cte per K (1/K)
0.000023
Density Kg M3 (kg/m3)
2,700
Elastic Modulus MPa (MPa)
73,000
Elongation Percent (%)
15
Heat Treatment
Wrought
Melting Point C (°C)
510
Name
Aluminum Alloy 2011-T3
Poisson Ratio (dimensionless)
0.33
Shear Modulus MPa (MPa)
26,000
Specific Heat J kgK (J/(kg·K))
864
Standard
ANSI
Tensile Strength MPa (MPa)
379
Thermal Conductivity W mK (W/(m·K))
151
Yield Strength MPa (MPa)
296

Source: ANSI