Explore the Engineering Database more efficiently by signing up for free. Sign up free

Aluminum-Alloy-1100-O — Aluminum Alloy

Category
Aluminum Alloy
Material Id
Aluminum Alloy 1100-O
Brinell Hardness (HB)
23
Cte per K (1/K)
0.000024
Density Kg M3 (kg/m3)
2,700
Elastic Modulus MPa (MPa)
73,000
Elongation Percent (%)
35
Heat Treatment
Wrought
Melting Point C (°C)
646
Name
Aluminum Alloy 1100-O
Poisson Ratio (dimensionless)
0.33
Shear Modulus MPa (MPa)
26,000
Specific Heat J kgK (J/(kg·K))
904
Standard
ANSI
Tensile Strength MPa (MPa)
90
Thermal Conductivity W mK (W/(m·K))
222
Yield Strength MPa (MPa)
34

Source: ANSI