Explore the Engineering Database more efficiently by signing up for free. Sign up free

Al-Li-8090-T8771-T-365K — Aluminum Alloy

Category
Aluminum Alloy
Material Id
Al-Li 8090 T8771 T 365K
Density Kg M3 (kg/m3)
2,600
Elongation Percent (%)
9.466667
Grade
8090-T8771
Heat Treatment
T8771
Name
Al-Li 8090-T8771 Transverse
Property Basis
Typical
Reduction Percent (%)
18.4
Specific Heat J kgK (J/(kg·K))
1,038
Standard
Nistir 3971
Tensile Strength MPa (MPa)
486.333333
Test Direction
Transverse
Test Temperature C (C)
91.85
Yield Strength MPa (MPa)
423.666667

Source: NISTIR 3971

aluminum_alloy — material id Al-Li_8090_T8771_T_365K · name Al-Li 8090-T8771 Transverse · tensile strength MPa 486.333 MPa · yield strength MPa 423.667 MPa · elongation percent 9.46667 % | Metal Alloy Properties | Engineering Database