Al-Li-8090-T8-T-255K — Aluminum Alloy

Category
Aluminum Alloy
Material Id
Al-Li 8090 T8 T 255K
Cte per K (1/K)
0.000021
Density Kg M3 (kg/m3)
2,600
Elongation Percent (%)
6.5
Grade
8090-T8
Heat Treatment
T8
Name
Al-Li 8090-T8 Transverse
Property Basis
Typical
Specific Heat J kgK (J/(kg·K))
930
Standard
Nistir 3971
Tensile Strength MPa (MPa)
529
Test Direction
Transverse
Test Temperature C (C)
-18.15
Thermal Conductivity W mK (W/(m·K))
71
Yield Strength MPa (MPa)
444.5

Source: NISTIR 3971