Al-2219-T87-L-75K — Aluminum Alloy
- Category
- Aluminum Alloy
- Material Id
- Al 2219 T87 L 75K
- Cte per K (1/K)
- 0.000017
- Density Kg M3 (kg/m3)
- 2,820
- Elongation Percent (%)
- 13.8
- Grade
- 2219-T87
- Heat Treatment
- T87
- Name
- Al 2219-T87 Longitudinal
- Property Basis
- Typical
- Reduction Percent (%)
- 23.8
- Specific Heat J kgK (J/(kg·K))
- 469
- Standard
- Nistir 3971
- Tensile Strength MPa (MPa)
- 581.6
- Test Direction
- Longitudinal
- Test Temperature C (C)
- -198.15
- Thermal Conductivity W mK (W/(m·K))
- 56
- Yield Strength MPa (MPa)
- 466.6
Source: NISTIR 3971