Al-2219-T851-L-20K — Aluminum Alloy
- Category
- Aluminum Alloy
- Material Id
- Al 2219 T851 L 20K
- Cte per K (1/K)
- 0.000014
- Density Kg M3 (kg/m3)
- 2,820
- Elongation Percent (%)
- 10.6
- Grade
- 2219-T851
- Heat Treatment
- T851
- Name
- Al 2219-T851 Longitudinal
- Property Basis
- Typical
- Reduction Percent (%)
- 17.2
- Standard
- Nistir 3971
- Tensile Strength MPa (MPa)
- 642.5
- Test Direction
- Longitudinal
- Test Temperature C (C)
- -253.15
- Yield Strength MPa (MPa)
- 429.5
Source: NISTIR 3971