Al-2219-T37-S-75K — Aluminum Alloy

Category
Aluminum Alloy
Material Id
Al 2219 T37 S 75K
Cte per K (1/K)
0.000017
Density Kg M3 (kg/m3)
2,820
Grade
2219-T37
Heat Treatment
T37
Name
Al 2219-T37 Short Transverse
Property Basis
Typical
Specific Heat J kgK (J/(kg·K))
469
Standard
Nistir 3971
Tensile Strength MPa (MPa)
525.5
Test Direction
Short Transverse
Test Temperature C (C)
-198.15
Thermal Conductivity W mK (W/(m·K))
56

Source: NISTIR 3971