R-1726 — Cellular Polystyrene Expanded
- Material Id
- Cellular Polystyrene Expanded
- Record Id
- 1726
- Date
- 12/11/1967
- Delta T (F)
- 24.36
- Delta X (in)
- 1.0177
- Density (lb/ft3)
- 1.875
- Description
- White pigment, Bead-Type
- Form
- Board
- K W Mk (W/mK)
- 0.2393
- Material
- Cellular Polystyrene, Expanded
- Mean Temp (F)
- 75.21
- R Value per Inch (ft2hF/BTU/in)
- 0.602707
- Rsi per Inch (m2K/W/in)
- 0.106143
- Standard
- Nist Srd 81 API
- Test Method
- ASTM C 177
Source: NIST SRD 81 API