Heat Treatment Parameters: nickel_superalloy
Heat treatment process parameters for engineering alloys — annealing, normalizing, quench-and-temper, precipitation hardening, carburizing, and stress relief. Covers carbon steels (1020/1045/1080), alloy steels (4130/4140/4340/8620/52100), tool steels (H13/D2/M2), stainless steels (304/316/17-4PH/15-5PH), aluminum alloys (2024/6061/7075), Ti-6Al-4V titanium, and Inconel 718. Per ASM Handbook Vol.4A/4B, ASTM A255, AMS 2770.
| alloy family | record id | alloy | hardness as treated HRC (HRC) | hold time min (min) | notes | temper temp max C (C) | temper temp max F (F) | temper temp min F (F) | treatment type |
|---|---|---|---|---|---|---|---|---|---|
| nickel_superalloy | Inconel718_DA | Inconel 718 | 1,080 | 1,325 | 1380 | 621 | 1,150 | 718 | direct_age |
This is a sample. Search the full heat treatment parameters dataset and 300+ more by creating a free account and accessing the database.