Frp Rebar Wrap Properties: CFRP_plate
Fiber-reinforced polymer (FRP) reinforcement properties for concrete structures — GFRP/CFRP/BFRP/AFRP bars per ACI 440.1R-15, and CFRP/GFRP/AFRP externally bonded wraps and pultruded plates per ACI 440.2R-17; includes tensile strength, elastic modulus, ultimate strain, density, CTE, bond strength, and environmental reduction factors CE
| product type | record id | bar size or width | density kg per m3 (kg/m3) | diameter mm or thickness mm (mm) | elastic modulus GPa (GPa) | environmental reduction factor CE | fiber type | notes | tensile strength MPa (MPa) | ultimate strain pct (%) |
|---|---|---|---|---|---|---|---|---|---|---|
| CFRP_plate | CFRP_plate_M | 50mm_wide | 1,600 | 1.2 | 210 | 0.85 | carbon_high_modulus | CFRP pultruded plate medium-modulus; Sika CarboDur M-type equivalent; E=210 GPa; f*fu=2400 MPa; thickness 1.2mm; used where higher stiffness desired for pre-stressed applications | 2,400 | 1.15 |
| CFRP_plate | CFRP_plate_S | 50mm_wide | 1,600 | 1.2 | 165 | 0.85 | carbon_standard | CFRP pultruded plate; Sika CarboDur S-type equivalent; width 50mm standard; thickness 1.2mm; E=165 GPa; f*fu=2800 MPa per Sika CarboDur S PDS; epoxy bonded to substrate; NSM or externally bonded; CE=0.85 (same as CFRP wrap per ACI 440.2R-17) | 2,800 | 1.7 |
| CFRP_plate | CFRP_plate_UHM | 50mm_wide | 1,700 | 1.4 | 400 | 0.85 | carbon_high_modulus | CFRP pultruded plate ultra-high modulus; Sika CarboDur UHM-type equivalent; E=400 GPa (pitch-based carbon); f*fu=1600 MPa; lower ultimate strain; used for stiffness-critical applications; thickness 1.4mm | 1,600 | 0.4 |