Explore the Engineering Database more efficiently by signing up for free. Sign up free
Home/Reference Data/Friction Coefficients/Teflon/Steel-1032-ASM-unlubricated

Steel-1032-Asm-Unlubricated — Teflon

Material 1
Teflon
Material 2 Condition
Steel 1032 Asm Unlubricated
Material 2
Steel, 1032
Mu Kinetic Max (dimensionless)
0.27
Mu Kinetic Min (dimensionless)
0.27
Mu Static Max (dimensionless)
0.27
Mu Static Min (dimensionless)
0.27
Surface Condition
Unlubricated, Room temperature, Ambient Air