Explore the Engineering Database more efficiently by signing up for free. Sign up free
Home/Reference Data/Friction Coefficients/Steel, Stainless/Cr2O3-plasma-sprayed-ASM-unlubricated

Cr2O3-Plasma-Sprayed-Asm-Unlubricated — Steel, Stainless

Material 1
Steel, Stainless
Material 2 Condition
Cr2O3 Plasma-Sprayed Asm Unlubricated
Material 2
Cr2O3, Plasma-Sprayed
Mu Kinetic Max (dimensionless)
0.15
Mu Kinetic Min (dimensionless)
0.14
Surface Condition
Unlubricated, Room temperature, Ambient Air
Steel, stainless — material 2 condition Cr2O3_plasma-sprayed_ASM_unlubricated · material 2 Cr2O3, plasma-sprayed · mu kinetic min 0.14 dimensionless · mu kinetic max 0.15 dimensionless · surface condition Unlubricated, room temperature, ambient air | Friction Coefficients | Engineering Database