Explore the Engineering Database more efficiently by signing up for free. Sign up free

Steel-1032-Asm-Unlubricated — Al, Alloy 6061-T6

Material 1
Al, Alloy 6061-T6
Material 2 Condition
Steel 1032 Asm Unlubricated
Material 2
Steel, 1032
Mu Kinetic Max (dimensionless)
0.25
Mu Kinetic Min (dimensionless)
0.25
Mu Static Max (dimensionless)
0.35
Mu Static Min (dimensionless)
0.35
Surface Condition
Unlubricated, Room temperature, Ambient Air
Al, alloy 6061-T6 — material 2 condition Steel_1032_ASM_unlubricated · material 2 Steel, 1032 · mu static max 0.35 dimensionless · mu static min 0.35 dimensionless · mu kinetic max 0.25 dimensionless | Friction Coefficients | Engineering Database