Elastomer Service Properties: HNBR

Service temperature limits, chemical resistance ratings, mechanical properties, and cure data for engineering elastomers and rubber compounds

Mechanical Engineeringelastomer: HNBR2 rows
elastomergrade or variantacid resistanceastm designationchemical resistance notescommon namecompression set pct (%)compression set temp Ccompression set time hrcure systemdensity g cm3 (g/cm3)elongation at break pct (%)fuel resistancegas permeabilityglass transition temp C (C)hardness range shore amax continuous temp C (C)max peak temp C (C)max service temp C (C)min service temp C (C)notesoil resistanceozone resistancesteam resistancetensile strength mpa (MPa)tr10 temp C
HNBRgeneralFairDH (ASTM D2000)Hydrogenated C-C double bonds give superior heat and ozone resistance vs NBR while retaining excellent oil resistance; high tensile and abrasion resistanceHydrogenated Nitrile<3015070peroxide1.30-1.40200-450GoodLow-25 to -2050-90165180165-40Zetpol (Zeon), Therban (LANXESS); used in automotive timing belts, oil field sealsExcellentGoodPoor20-31-35 to -30
HNBRhigh_satGoodDH (ASTM D2000)Near-fully saturated backbone; maximum ozone and heat resistance; used in dynamic applications requiring long service lifeHNBR High Saturation (>99%)15-2515070peroxide1.30-1.40200-400GoodLow-25 to -1860-90150170150-35Therban XT or Zetpol 2000 class; saturation >99%ExcellentExcellentPoor20-31-30 to -25

This is a sample. Search the full elastomer service properties dataset and 300+ more by creating a free account and accessing the database.

Get started for FREE

Related data