Seawater-25C — Super Duplex 2507

Metal Id
Super Duplex 2507
Environment Id
Seawater 25C
Concentration Pct (%)
3.5
Corrosion Rate MM Yr (mm/yr)
0.0005
Corrosion Rate Mpy (mpy)
0.02
Crevice Corrosion Risk
Low
Environment Description
Seawater (3.5% NaCl)
Metal Name
Super Duplex 2507 (UNS S32750)
Pitting Potential MV (mV)
550
Pren
43
Resistance Rating
Excellent
Stress Corrosion Risk
Low
Temperature C (C)
25
super_duplex_2507 — environment id seawater_25c · environment description Seawater (3.5% NaCl) · corrosion rate mm yr 0.0005 mm/yr · corrosion rate mpy 0.02 mpy · resistance rating excellent | Corrosion Rates | Engineering Database