Seawater-25C — Inconel 625

Metal Id
Inconel 625
Environment Id
Seawater 25C
Concentration Pct (%)
3.5
Corrosion Rate MM Yr (mm/yr)
0.0005
Corrosion Rate Mpy (mpy)
0.02
Crevice Corrosion Risk
Low
Environment Description
Seawater (3.5% NaCl)
Metal Name
Inconel 625 (UNS N06625)
Pitting Potential MV (mV)
750
Pren
51
Resistance Rating
Excellent
Stress Corrosion Risk
Low
Temperature C (C)
25