Explore the Engineering Database more efficiently by signing up for free. Sign up free

HNO3-10PCT-25C — 316 SS

Metal Id
316 SS
Environment Id
HNO3 10PCT 25C
Concentration Pct (%)
10
Corrosion Rate MM Yr (mm/yr)
0.008
Corrosion Rate Mpy (mpy)
0.3
Crevice Corrosion Risk
Low
Environment Description
Nitric Acid 10% at 25°C
Metal Name
AISI 316 Stainless Steel (UNS S31600)
Pren
24.5
Resistance Rating
Excellent
Stress Corrosion Risk
Low
Temperature C (C)
25
316_ss — environment id hno3_10pct_25c · environment description Nitric acid 10% at 25°C · corrosion rate mm yr 0.008 mm/yr · corrosion rate mpy 0.3 mpy · concentration pct 10 % | Corrosion Rates | Engineering Database