R-480 — 200

Pressure Bar
200
Temp K
480
Cp kJ kgK (kJ/kgK)
1.3671
Density Kg M3 (kg/m3)
252.21
Enthalpy kJ Kg (kJ/kg)
607.22
Entropy kJ kgK (kJ/kgK)
2.0663
Fluid
CO2
Phase
Supercritical
Specific Volume M3 Kg (m3/kg)
0.00396
Thermal Conductivity W mK (W/mK)
0.04261
Viscosity uPa S (uPa*s)
28.932
200 — temp K 480 · thermal conductivity W mK 0.04261 W/mK · specific volume m3 kg 0.00396 m3/kg · entropy kJ kgK 2.0663 kJ/kgK · viscosity uPa s 28.932 uPa*s | Co2 Superheated | Engineering Database