70-Ti-6AL-6V-2SN-Extrusion-Ann-2.000-B — Ti-6AL-6V-2SN Extrusion Ann

Material Id
Ti-6AL-6V-2SN Extrusion Ann 2.000 B
Temp F
70
E Msi (Msi)
16
Ec Msi (Msi)
16.4
Fbru Ksi (ksi)
229
Fbru Ksi 2 (ksi)
281
Fbry Ksi (ksi)
203
Fbry Ksi 2 (ksi)
235
Fcy Ksi (ksi)
144
Fcy Ksi Lt (ksi)
142
Fsu Ksi (ksi)
97
Ftu Ksi (ksi)
148
Ftu Ksi Lt (ksi)
148
Fty Ksi (ksi)
135
Fty Ksi Lt (ksi)
135
G Msi (Msi)
6.2
Basis
B
Condition
Annealed
Density Lb IN3 (lb/in^3)
0.164
Form
Extruded Bar and Shapes
Poisson Ratio
0.31
Specification
MIL-T-81556 & AMS-T-81556, Comp. Ab-3
Thickness Range
2.000
TI-6AL-6V-2SN EXTRUSION ANN — temp f 70 · material id TI-6AL-6V-2SN_EXTRUSION_ANN_2.000_B · Fcy ksi 144 ksi · Fcy ksi LT 142 ksi · Ftu ksi 148 ksi | Aerospace Materials | Engineering Database