Explore the Engineering Database more efficiently by signing up for free. Sign up free
Home/Reference Data/Aerospace Materials/7050 Forging T7452/70-7050-FORGING-T7452-2.001-3.000-S

70-7050-Forging-T7452-2.001-3.000-S — 7050 Forging T7452

Material Id
7050 Forging T7452 2.001-3.000 S
Temp F
70
E Msi (Msi)
10.2
Ec Msi (Msi)
10.6
Fbru Ksi (ksi)
97
Fbru Ksi 2 (ksi)
129
Fbry Ksi (ksi)
84
Fbry Ksi 2 (ksi)
100
Fcy Ksi (ksi)
62
Fcy Ksi Lt (ksi)
63
Fcy Ksi St (ksi)
63
Fsu Ksi (ksi)
41
Ftu Ksi (ksi)
72
Ftu Ksi Lt (ksi)
70
Ftu Ksi St (ksi)
67
Fty Ksi (ksi)
62
Fty Ksi Lt (ksi)
60
Fty Ksi St (ksi)
55
G Msi (Msi)
3.9
Basis
S
Condition
T7452
Density Lb IN3 (lb/in^3)
0.102
Elongation Pct (%)
9
Elongation Pct Lt (%)
5
Elongation Pct St (%)
4
Form
Hand Forging
Poisson Ratio
0.33
Specification
AMS 4108 and AMS-a-22771
Thickness Range
2.001-3.000
7050 FORGING T7452 — temp f 70 · material id 7050_FORGING_T7452_2.001-3.000_S · Fbry ksi 2 100 ksi · Fbry ksi 84 ksi · Fbru ksi 2 129 ksi | Aerospace Materials | Engineering Database