| material process | condition | alloy | density relative pct (%) | elongation pct xy (%) | elongation pct z (%) | hardness HRC (HRC) | max service temp C (C) | modulus GPa (GPa) | notes | powder size um (um) | process | surface roughness Ra um (um) | tensile strength MPa xy (MPa) | tensile strength MPa z (MPa) | yield strength MPa xy (MPa) | yield strength MPa z (MPa) |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| inconel718_ded | as_built | Inconel 718 | 99 | 25 | 18 | 28 | 650 | 200 | DED directed energy deposition; coarser microstructure; lower strength than SLM; near-net shape large parts | 100 | DED | 50 | 950 | 900 | 700 | 650 |